产品介绍       |       联系我们       |       公司简介




产品搜索
   
 





 产品介绍-》慕湖产品


3004聚氨酯防水涂料
Polyurethane waterproof coation

一、产品介绍 Introduction of product
   环保型聚氨酯防水涂料是焦油聚氨酯防水涂料的升级换代产品分为单组份和双组份两类。涂料在施工涂覆后,经过化学反应固化后,形成坚固耐用无缝弹性胶膜, 它具有整体性能好、抗拉强度大、延伸率高、弹性好、粘结力强、耐高低温耐老化、无污染、冷施工、维修方便等特点。
   Polyurethane waterproof coating of Environmental protection type is the escalation of tar-polyurethane waterproof coating. It includes two types: two-component and one-component. Affer the coating was smeared, it will become firm solid. The product has good functions : good tensil strength, high flexibility, high viscosity, resistant to aging at high and low temperature ture and non-pollution as well as cool-construction etc.

二、适用范围 Application scope
   适用于屋面、 地下室及厨房、 厕浴间等建筑防水工程地铁、隧道、水渠、游泳池、不规则的混凝土及木结构防水。
   Used in the roofing of the building, underhouse, toilet, tunnel and subway.

三、技术指标 Physical performance

项 目 Item

指标, Index

拉伸强度 Mpa(tensil Strength , Mpa)

>1.65

延伸率 (elongation)

>350

固体含量% (proportion of solid, % )

≥ 94

低温柔性 - 30 ℃ (resistant to low temperature -30 ℃ )

无裂缝 (NO fissure)

不透水性: 0.3Mpa , 30min(resistant to water , 0.3Mpa , 30min)

不渗漏 (NO permeation)

涂膜表干时间 h(the time of the surface to be arid)

≤ 4 不粘手

涂膜实干时间 h(the time of the coating to be arid)

≤ 12 无粘着

四、施工要点 Construction point
   1 、基础要求干净、坚固、干燥、无明水、有裂缝应先用涂料进行修复封闭。
   2 、用橡胶刮板将涂料均匀地涂刮在地面上,要保证涂层厚度达到设计要求, 不应有漏洞、起鼓、离层等现象,落水管和伸缩缝的施工要用玻纤布作加强层。
   3 、涂层干固时间常温下约 12 小时,普通防水施工,涂层厚度应在 1.2mm 左右,重要的防水工程需涂刮 2~3 次,每次涂覆的时间间隔以前一次不粘手为准。如需做保护层,可在涂料未固化前,在其表面上粗沙,可使保护层和防水层之间粘结牢固。
   4 、对金属板、管材的防腐施工要求先进行除锈、清洗处理后再进行涂料施工。
   5 、使用参考如图:
   The base should be clean, firm , dry and no water . If you find the fissure, please use the coating to seal it before construction.
   Using rubber-scraper to smear the coating on the floor, please assure that the thickness is suitable . It should not have leak, air and break on the surface.
   Please to wind the glass fibre cloth on the water pipe before smearing the coating.
   After 12 hours during ordinary temperature the coating would to be solid, The coating thickness should to be about 1.2mm for the common construction.
   The coating should to be smeared 2-3 times for the important construction . When the surface of the coating is not gluey, you can smear new coating . To sprinkle the rough sand on the coating surface before the coating becomes sold, so that you can get a protection layer.

The construction of the metal and pipe should ablate the rust first.

涂层厚度 mm

Thickess

参考用量 kg/m 2

Reference weight of using

涂覆次数 Smearing time

使用范围

Application scope

1.0

1.2-1.4

一遍

一般建筑物天面、地下室、防水装饰

Covering of building , underhouse, waterproof ornament etc .

1.5

1.8-2.0

二遍

重要等级防水、管口、伸缩缝、防水装饰

Important water-proof, pipe and waterproof ornament

2.0

2.5

二至三遍

加强型防水装饰 Stengthened type waterproof ornament

五、注意事项 Attention
   1 、建议一次用完,当产品贮存期较长时,涂料表面会形成一层薄胶膜,使用时剔除,不影响使用效果。
   2 、本产品基本颜色为浅灰色。
   3 、本产品应贮存在室内阴凉处,并注意密封防潮,贮存与运输过程中避免与水接触,远离火源,保质期一年。
   4 、施工环境要通风良好。

Pay attention to :
   A. To use the coating one time, When the product was stored a long time, it would has a film of rubber on the surface. You can ablate the film when constructing.
   B. The basic colour of the product is light-grey.
   C. The sealed product should be stored in the shade. In the order of keeping and transporting, the product should avoid water and fire. The service life of the coating is one year.
   D. The environment of construction should be in good ventilation.

六、产品应用
  
非焦油聚氨酯防水涂料(沥青基)是一种新型防水涂料。它是一种双组份反应型固化成膜的高分子防水涂料。产品无毒,对环境无污染,防水性能良好,被国家建设部推荐使用的十三种防水材料之一。甲组分是带有-NCO基团的聚醚预聚物,乙组分是以沥青基填料、固体填料、表面活性剂、固化剂、催化剂等含有-OH和-NH2基团的灰色或其他色彩的稠状液。使用时,将甲、乙两组分按1∶2的比例混合,经数小时后固结成既富有弹性、坚韧又有耐久性的整体涂膜防水层。非焦油聚氨酯防水涂料(沥青基)产品根据需要可生产灰色或深色色彩产品。用于地下室、新旧屋面、卫生间、桥梁、涵洞、人防工程等场合的防水、防潮、也可用于金属管道、车间地坪、水池等防腐蚀使用。
七、主要特点
  
涂膜层具有橡胶的特性,延伸性大,富有弹性,能适应基层微量变形,耐热老化、耐腐蚀、水密性高、防水性能极佳;施工周期短,维修容易;冷作业施工,常温固化,操作方便,涂层整体无接缝,防水效果好;具有较好的自粘性,适宜旧屋面的返修,新老涂层能融为一体,不脱层;附着力强,对混凝土基面、木材、金属、陶瓷表面有极强粘附力;延伸性大、不起泡、不起壳,特别适宜于屋面隔气层、厨卫间、地下工程的防水。
  优异的力学性能,低温性能,施工方便,涂膜无接缝、良好的粘结性、维修简便快捷。绿色环保,固含量高。对基面含水率适应性强,可在较潮湿的基面上施工,也可在相对湿度较大的条件下施工。不需要现场配料,省时省工,不会发生计量差错而影响质量
八、产品标准
  
GB/T19250—2003《聚氨酯防水涂料》,GB50325—2001《民用建筑工程室内环境污染控制规范
九、性能指标

型号

拉伸强度(MPa)

断裂伸长率(%)

固含量(%)

低温柔性

不透水性

≥ 1.90

≥ 550

≥ 80

-40度,2H 无裂纹

0.3MPa ,30min 不透水

≥ 2.45

≥ 450

﹡注:产品复试时,涂膜分多遍成形,每遍成膜厚度不超过0.3mm为宜
十、施工方法
1基层处理:要求表面平整、结实,无浮砂,无明水。
2物料搅拌均匀后用刷子或像胶刮板刮涂,打底。
3涂刷表面:底层固化后,分多层涂刷面层,每遍0.3~0.4mm厚,每遍刮涂与上一次方向垂直以使涂膜厚度均匀,直至厚度达到设计要求。
4稀撒石渣:如果用于立面施工,应在最后一层涂料涂抹完毕但尚未完全固化时,在其表面稀撒上少量干净的2~3mm厚的石渣,以增加涂膜和水泥砂浆的粘结力。
5当涂膜完全固化和验收合格后,即可做水泥砂浆保护层或用传统方法贴面砖、马赛克等。
十一、涂膜验收
  
在做保护层前必须认真检查涂膜防水层的施工质量,要满涂不断,薄厚均匀一致,并且达到设计要求厚度,封闭严密,不允许有露见白、起鼓脱落、开裂翘边等缺陷存在,必要时还可 24h蓄水检查,至不渗漏为合格。
十二、注意事项
1、涂刷面层时,每遍不宜过厚,否则涂膜容易起泡。
2、施工现场必须保持良好的通风。
3、请按照桶包装上标明的宜用时间使用。
十三、参考用量:1.5kg~2.5kg/㎡
十四、包装及贮存
  
20kg/桶、 5kg/桶包装。储存温度5℃~35℃,避免长时间阳光直射,物料绝对禁止与水接触,存放现场严禁烟火。保质期为6个月。



北京慕湖外加剂有限公司 版权所有
Copyright©2001 Beijing Muhu Concrete Admixture Co.,Ltd.
通用网址:慕湖 慕湖外加剂 砼外加剂
设计制作:
中国建材电子商务网